Switching from High Lead Solders to Eutectic AuSn
Two categories of solder are available to choose from when the in-service environment for a device reaches above 125°C either in continuous operat...
Two categories of solder are available to choose from when the in-service environment for a device reaches above 125°C either in continuous operat...
Indium Corporation is hosting a booth (#809) and will be highlighting a series of......
Indium and indium-containing alloys see wide use in a multitude of soldering applications. Indium has many attractive properties such as remaining duc...
Folks, I’m taking a few moments from Wassail Weekend , held annually in my village, Woodstock VT, “The prettiest small town in Americ...
Here is a question that was received and answered on our website almost a decade ago – but it is still quite relevant: p......
Following on from our discussions of last time... As you will recall from the previous post on this topic, My friend and colleague Chris Nash and I w...
My friend and colleague Chris Nash and I were recently discussing some puzzling results for low dip height found during testing of package-on-pac...
If you have ever handled a piece of 80Au 20Sn solder alloy, one of the things that......
Dr Ning-Cheng Lee (Indium Corporation‘s Vice-President of Technology) just let me review his team’s excellent upcoming paper on solde...
Solder wire is generally used for manual soldering operations, including rework. But, it can......
Many, many thanks to the hundreds of you who came by the Indium Corporation booth at Semicon West this year. Some of you came to hear about ...