Improved Solder Density and Solder Paste Volume Fraction Tool
Folks, It is hard to believe that I have been blogging for over 7 years now. In all this time it has surprised me how much interest there has be...
Folks, It is hard to believe that I have been blogging for over 7 years now. In all this time it has surprised me how much interest there has be...
Individually, indium and gallium each have some pretty interesting characteristics. Gallium is liquid at 30°C (86°F) and, because it is less t...
Folks, There is a lot of interest in cleaning PCBs that have been assembled with no-clean solder pastes. Recently I discussed the topic with my ...
Browse the coming attractions at your local movie theater. How many 3D movies are being advertised? 3D is a very exciting technology for m...
Folks, In Ken Burn’s excellent miniseries The Civil War, Shelby Foote states that the Civil War made us a country by uniting No...
Okay, I have to admit I was wrong… I used to have a bias against L-Shaped bus ribbon. “Why not just use available continuously spooled ri...
While it is important to have at least 10µm of solder on each side of a tabbing ribbon to form a proper solder joint during cell interconnection...
Folks, If you need to take a break from topics such as solder paste, solder preforms, tin whiskers, indium TIMs etc, there are a few books I would r...
It is not often that we get a request for SIR (Surface Insulation Resistance) and/or ECM (Electro-Chemical Migration) results for a water washable/sol...
A few months back, while discussing tricks for hand soldering c-Si solar cells, I mentioned flux . One tip I didn’t mention is how to APPLY......
Folks, Struggling to find a good, royalty-free, video of electronics assembly, my Dartmouth ENGM 185 class on manufacturing processes decided t...
Indian electronics manufacturers and solder users. This info is for you. After many years of discussion and policy making, the Indian Government rolle...