Which Off-Eutectic AuSn Alloy Do I Use?
Plating dies and/or substrates with pure gold works well to prevent the components from oxidizing, but can lead to undesirable gold-rich solder joints...
Plating dies and/or substrates with pure gold works well to prevent the components from oxidizing, but can lead to undesirable gold-rich solder joints...
Performing die-attach using AuSn solder alloy preforms against gold plating? You may need an off-eutectic solder alloy to compensate for the Au that i...
Adding Indium Corporation's Solder Fortification to edge connectors within mobile devices improves reliability by strengthening the solder joint....
Using gold-tin solder in high-temp applications for both high-temperature and LED applications, there's been an increase in voiding which may corr...
Gold-plated surfaces are widely used in electronics assembly, but using common tin-based solder alloys can scavenge the gold. There's a better sol...
Here’s a true story regarding the service temperature of solder joints. Yesterday, as I left work, I noticed that it felt really hot outside. I ...
Solder joint voiding is tough to deal with. When attaching components, such as power amplifiers/transistors or QFNs, the larger the footprint the...
It is often said that a chain is only as strong as it weakest link, the same can be true for a series of......