Solder Troubleshooting

Posted by Amanda M. Hartnett
March 12th, 2008

Why doesn’t my solder flow?


The most common issue preventing good solder wetting on a substrate is oxidation. All metals are prone to some level of surface oxide formation when exposed to ambient conditions. Solders cannot wet substrates when they or the substrate they are soldering to is oxidized.


How can I be sure that oxidation is my problem? Well, is your solder balling up on the surface like the water droplet shown in this image? If so, you have an oxidation problem.


How do I remove this oxidation? Indium has over fifty fluxes formulated for removing oxides. Every Indium technical staff member is trained to identify the appropriate flux to suit your application and will be happy to do so. Feel free to contact us here.


Can’t use a flux? Other oxide removal techniques include chemical etches, plasma cleaning, ultrasonic soldering, or use of a reducing atmosphere.


image courtesy of www.malawicichlidhomepage.com

Posted by Amanda M. Hartnett on March 12th, 2008 at 1:25 PM

Comments (add your comment)

    There are no comments on this entry yet.

Comment on this entry

optional (will not appear online)
http://yoursite – optional (will appear online)

Important! Please find the letters in the image opposite, then type them into the box above. You are asked to do this in order to verify that this comment is not being submitted by an automated process.

top of page