1) Pot your sample with enough epoxy that you can comfortably hold the sample.
1) Start with a fresh piece of sandpaper every time. You don’t know how the last person [mis]used it.
2) Don’t skip over intermediate grits. The intermediate grit paper is there for a reason – and it doesn’t save any time or effort to go from 80 grit to 600 grit.
3) Wash the sample after every step, so you don’t transfer larger grits to finer paper
4) Make a sample your proud of. I like to polish both sides and the perimeter of the samples I am working with, if I have time. This is impressive when sent back to a customer, or it can be used as a display at a trade-show.

Posted by Jim Hisert on January 30th, 2008 at 9:52 AM

Comments (add your comment)

    There are no comments on this entry yet.

Comment on this entry

optional (will not appear online)
http://yoursite – optional (will appear online)

Important! Please find the letter in the image opposite, then type it into the box above. You are asked to do this in order to verify that this comment is not being submitted by an automated process.

top of page