Amigos,
Digikey colleague Aaron Rollens developed the equation to convert the mass on a spool of solder wire into its length. I also developed the equation to convert a length of solder wire into its mass.
These equations are below in Figure 1.

Figure 1. The Equations for Converting Wire Mass to Lenth and Vice Versa.
Being an Excel® nerd, I decided to develop an Excel® spreadsheet that would calculate the length or mass in these equations. An image of the spreadsheet is in Figure 2.

Figure 2. The Excel Spreadsheet to Perform the Calculations
These calculations and spreadsheet only work for solid wire, they will not work for flux core wire.
If you would like a copy of the spreadsheet send me an email at [email protected].
Salud,