용융성 합금/저융점 합금

Fusible alloys, known for their lower melting points compared to solder alloys, are easily liquefied with moderate heat, making them ideal for temporary solid state during processing or as temperature sensors, such as in fire detection sprinkler systems. Originally developed in the 19th century and known by names such as Field’s metal, Wood’s metal, and Rose’s metal, these alloys have evolved with modern materials technology to include precise compositions like Indalloy®117, Indalloy®158, and Indalloy®19, delivering consistent melting behavior across an extended temperature range.

Indium Corporation 제공

  • Broad Alloy Portfolio and Formulation Depth
  • Materials Science and Process Support
  • Leading Global Supplier of Fusible Alloys
Lens Blocking using Fusible Alloys
Lens Blocking using Fusible Alloys or Low Melting Point Alloys

제품 개요

Fusible alloys, characterized by their low melting points as low as 47°C (117°F), offer remarkable versatility by transitioning seamlessly between solid and molten states. This unique property makes them indispensable for precise and temporary applications. These alloys serve as excellent as precision support materials, securely holding and protecting workpieces during crucial finishing processes, such as polishing and grinding. Additionally, the eutectic melting points of fusible alloys facilitate passive activation systems, ensuring the reliable and safe operation of devices like fire sprinklers without the need for electronic circuitry, thereby enhancing safety and simplicity.

사용 가능한 합금 구성의 최대 범위

Field’s metal, Wood’s metal, and many other alloy compositions are available. Available melting points start at 47°C/117°F and go up into the solder alloy range at above 200°C.

Lens Blocking for Grinding and Polishing with Indalloy®117 & Indalloy®19

Indalloy®117 and Indalloy®19 are the most popular alloys for lens blocking in the optical lens grinding industry, with melt points at 47°C/117°F and 60°C/140°F, respectively.

화재 스프링클러 시스템의 정확한 작동

Melting activation is solely controlled by environmental temperature and thus enables the design of completely passive devices for fire detection. Indalloy®158 is a popular alloy choice for fire sprinkler systems.

Custom Alloy Development

Melting behavior is determined by precise control of the alloy composition. We offer a wide range of alloy options and melting points. We also work with customers to develop custom alloys with target melting points and other properties tailored to their application needs.

Indalloy®117

Indalloy®19 (Field’s Metal)

Indalloy®158 (Wood’s Metal)

납 및 카드뮴 무함유 합금 옵션

인돌리 #11713619158281
합금 구성44.7 Bi
22.6 Pb
19.1 In
8.3 Sn
5.3 Cd
49 Bi
21 In
18 Pb
12 Sn
51 In
32.5 Bi
16.5 Sn
50 Bi
26.7 Pb
13.3 Sn
10 Cd
58 Bi
42 Sn
리퀴더스(°C(°F) 단위)47 (117)58 (136)
60 (140)

60 (140)

138 (281)
E = 유텍EEEEE

관련 애플리케이션

용융성 합금/저융점 합금은 다양한 용도에 적합합니다.

인쇄 회로 기판의 마이크로칩

PCB 어셈블리

Proven and cutting-edge materials for PCB assembly…

고온 납땜

고온 납땜

Offering high-temperature soldering materials for critical applications…

상단에 3개의 흰색 직사각형 라벨이 있는 극저온 봉인이 있는 검은색 질감의 실린더입니다.

밀봉: 극저온 및 완전 밀폐

Low temperature liquid & fusible alloys for…

관련 시장

인디엄 코퍼레이션의 용융성 합금/저융점 합금은 다양한 시장에 적합합니다.

기술적인 질문이나 영업 관련 문의 사항이 있으신가요? 전담 팀이 도와드리겠습니다. "한 엔지니어에서 다른 엔지니어로®"는 단순한 모토가 아니라 탁월한 서비스를 제공하겠다는 약속입니다. 언제나 준비가 되어 있습니다. 지금 바로 연락하세요!

이 이미지의 alt 속성은 비어 있으며 파일 이름은 과학자-현미경-with-microscope.png입니다.

안전보건자료를 찾고 계신가요?

기술 사양부터 애플리케이션 안내까지 필요한 모든 것을 한 곳에서 편리하게 이용할 수 있습니다.