Backward compatible with existing Sn/Pb processes - making it an excellent Pb-Free conversion flux
VOC-Free
Compatible with both Sn/Pb and Pb-Free wave soldering processes
Alcohol-based
Excellent hole fill and minimal solder balls
Enhanced long-term reliability (due to presence of rosin in formulation)
Accommodates long, hot preheat conditions
Slightly reduced activity and solids content to accommodate wide variations in flux application quantity
Can be qualified in an existing Sn/Pb process then used after the transition to a Pb-Free wave soldering process
Will continue delivering superior performance under the increased process temperatures for Pb-Free