Indium Corporation will introduce its new Indium Oxide High BET powder designed to support emerging applications of the display industry at SVC TechCon from May 5-10 in Orlando, Florida, USA.

Indium Corporation’s Indium Oxide High BET powder is designed for use in both display electrodes and thin-film oxide transistors as part of the transparent conductive oxide (TCO) film stack.

Indium Oxide High BET powder offers:

  • BET range from 13–17m2/g
  • Higher than 4N5 purity
  • Primary particle size between 50–100nm

This material supports the evolving needs of sputtering target production lines that need flexibility and the ability to scale in today’s fast-changing environment.

Indium Corporation’s reclaim capability includes a fully integrated manufacturing reclaim loop that provides a fast return-to-process time for our customers to lower inventory costs.

Visit us at booth #417 or find more information about our Indium Oxide products at http://www.indium.com/inorganic-compounds/indium-compounds/indium-oxide.

For more information about Indium Corporation, visit www.indium.com or email abrown@indium.com. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.