Liquid Flux Selector Kit

Liquid Flux Selector Kit

When you select your wire or ribbon kit you have a choice of 5 of the following flux types:

Indalloy Flux   Effective Temperature Range   Clean Residue In  
1 100 - 338°C Water
2 100 - 371°C Water
3 96 - 343°C Water
4 OA 100 - 250°C Water
5RA 125 - 350°C IPA
5RMA 125 - 350°C IPA
5R 125 - 350°C IPA

Below is a chart to help you choose the correct fluxes:

Indalloy Flux Metal to be soldered
1 Iconel/Monel/Zn/Mild Steel
2 Stainless Steel/High Chrome Super Steel, Nitinol
3 Al
4 OA SnNi electro deposit/Kovar
4 OA or 5RA Pb/Oxidized Cu
4 OA or 5RA Brass/Bronze/BeCu
4 OA or 5RA Rh/Cd
4 OA or 5RA Ni
5RA or 5RMA Solder Plate
5RA or 5RMA Sn
5R or 5RMA Clean Cu
5R or 5RMA Pt/Pd
5R or 5RMA Ag
5R or 5RMA Au

Also see Flux and Solder Compatibility in the technical section under application notes for more information.