Solder Alloy Ribbon Selector Kit

Click Here to Buy This Product Online at Buy.Solder.Com 

When creating your Ribbon Alloy Selector Kit, you can choose 3, 6, or 12 different alloys of 1.00" (25.4mm) x 0.002" (0.05mm) x 3 ft. (914mm) ribbon. Ribbon can be Solder Alloy Ribbon Selector Kitcut into experimental preforms (knife included) to determine the proper configuration. Solder volume can be increased by stacking cut preforms. Kits also come with several fluxes which can be found in the section on Liquid Flux Selection.

Choose from the following alloys ranging in temperature from 118°C to 312°C; included are Pb-Free, standard tin-lead, and indium-based solders. If your application involves non-metal bonding, refer to recommendations in the Wire Alloy Selector Kit: Non-Metal Bonding Selections. Spools are individually packed in argon-filled bags.

 

 

 

Indalloy Number Alloy Temperature (°C)
1E 52In 48Sn 118 E
2 80In 15Pb 5Ag 154 - 149
4 100In 157 MP
104 Sn62 62Sn 36Pb 2Ag 179 E
106 Sn63 63Sn 37Pb 183 E
121 96.5Sn 3.5Ag 221 E
150 81Pb 19In 275 - 260
151 92.5Pb 5Sn 2.5Ag 296 - 287
205 60In 40Pb 181 - 173
241 SAC387 95.5Sn 3.8Ag 0.7Cu 220 - 217
246 SAC405 95.5Sn 4Ag 0.5Cu 225 - 217
256 SAC305 96.5Sn 3Ag 0.5Cu 220 - 217
281 58Bi 42Sn 138 E
282 57Bi 42Sn 1Ag 140 - 139
290 97In 3Ag 143 E