Wire Selector Kit

You can select from the following alloys to determine the ideal solder for your application. Whether your application calls for lead free, low temperature or high temperature, the alloys listed below will help in the selection process. Personalize your kit with 2, 5, or 10 different alloys. Pricing is based on the number of alloys selected. Kits also come with several fluxes - for a complete list go to Liquid Flux Selector Kit.

For assistance in determining the correct solder to use with a metallization, you can reference our Application Note on Flux and Solder Compatibility or contact our Technical Support Engineers.

Liquidus temperatures range from 96°C to 300°C and include numerous lead-free alloys. These solders are popular for microelectronics and aerospace applications. In applications that require soldering to gold, use indium based alloys for service temperatures below 125°C. For service temperatures above 125°C, Indalloy 182 (80Au/20Sn) is recommended.


Indalloy # Alloy Temperature
(°C)
Pb-Free
1E 52In 48Sn 118 E X
2 80In 15Pb 5Ag 154 - 149  
3 90In 10Ag 237 - 143 X
4 100In 157 MP X
7 50In 50Pb 210 - 184  
9 70Sn 18Pb 12In 167 - 154  
42 46Bi 34Sn 20Pb 96 E  
104 Sn62 62Sn 36Pb 2Ag 179 E  
106 Sn63 63Sn 37Pb 183 E  
121 96.5Sn 3.5Ag 221 E X
133 95Sn 5Sb 240 - 235 X
136 49Bi 21In 18Pb 12Sn 58 E  
151 92.5Pb 5Sn 2.5Ag 296 - 287  
164 92.5Pb 5In 2.5Ag 310 - 300  
182 80Au 20Sn 280 E X
201 91Sn 9Zn 199 E X
204 70In 30Pb 175 - 165  
205 60In 40Pb 181 - 173  
241 SAC387 95.5Sn 3.8Ag 0.7Cu 220 - 217 X
244 99.3Sn 0.7Cu 227 E X
246 SAC405 95.5Sn 4Ag 0.5Cu 225 - 217 X
256 SAC305 96.5Sn 3Ag 0.5Cu 220 - 217 X
281 58i 42Sn 138 E X
282 57Bi 42Sn 1Ag 140 - 139 X
290 97In 3Ag 143 E X