Color | Acid Value | S.G. 25°C | S.G. 15°C | Solids Content | Flash Point | J-STD-004 Flux Type |
---|---|---|---|---|---|---|
Amber | 18 | 0.795 | 0.804 | 3.63 | 54 | ROL1 |
Oxidation | |
Icicles | |
Electro Migration | |
Residue | |
Skips & Bridges | |
Corrosion |
Color | Acid Value | S.G. 25°C | S.G. 15°C | Solids Content | Flash Point | J-STD-004 Flux Type |
---|---|---|---|---|---|---|
Amber | 14.4 | 0.796 | 0.802 | 5.77 | 54 | ROL0 |
Oxidation | |
Icicles | |
Electro Migration | |
Residue | |
Skips & Bridges | |
Corrosion |
Color | Acid Value | S.G. 25°C | S.G. 15°C | Solids Content | Flash Point | J-STD-004 Flux Type |
---|---|---|---|---|---|---|
Pale | 26.25 | 0.796 | 0.803 | 4.71 | 54 | ORL0 |
Oxidation | |
Icicles | |
Electro Migration | |
Residue | |
Skips & Bridges | |
Corrosion |
Color | Acid Value | S.G. 25°C | S.G. 15°C | Solids Content | Flash Point | J-STD-004 Flux Type |
---|---|---|---|---|---|---|
Clear | 28.5 | 0.798 | 0.805 | 4.99 | 12 | ORM0 |
Oxidation | |
Icicles | |
Electro Migration | |
Residue | |
Skips & Bridges | |
Corrosion |