Indium Corporation®
Select an area to search
  • People
    • Technical Support Engineers
    • Sales
    • Human Resources
      • Jobs
      • Community Support
    • Marketing Communications
      • Trade Shows
      • Company News
      • Corporate Awards
      • Technical Milestones
      • Social Media
    • Employee Biographies
    • Corporate
      • About Us
      • Social Responsibility
      • Company News
      • Corporate Awards
      • ISO and ITAR
      • Trade Shows
      • Corporate Literature
    • Bloggers
    • Social Media
    • Facilities
    • Contact Us
  • Products
    • Flux and Epoxy
      • Ball-Attach Flux
      • Epoxy Flux
      • Flip-Chip Flux
      • Flux Pens
      • Flux-Cored Wire
      • Industrial Flux
      • Liquid Tabbing Flux
      • Package-on-Package Flux
      • Tacky Flux
      • TCB and Copper PIllar Flux
      • Wave Flux
      • Wafer Bumping Flux
    • Inorganic Compounds
      • Featured Products
      • Indium Compounds
      • Gallium Compounds
      • Germanium Compounds
    • Metals
      • Indium
      • Gallium
      • Tin
      • Germanium
      • Reclaim and Recycle
    • NanoFoil®
      • Sheets
      • Preforms
      • Powders and Particles
      • Sputtering Target Bonding
    • Reclaim and Recycle
      • Metals Recycling
      • Solder and Solder Dross Recycle Program
    • Solar Assembly Materials
      • Metallization Paste
      • SUNTAB™ PV Ribbon
      • Liquid Tabbing Flux
      • Solders
    • Solder Paste and Powders
      • SACM™
      • Indium8.9 Series
      • Lead-Free
      • Tin-Lead
      • Package-on-Package Paste
      • Low Temp/High Temp
      • Die-Attach
      • Wafer Bumping Paste
      • Solder Fortification®
      • Gold-Based Solder Paste
    • Solders
      • Bismuth Solders
      • Gold Solders
      • Indium Solders
      • Bar Solder
      • Low Temp/High Temp
      • Preforms
      • Ribbon and Foil
      • Solder Fortification®
      • Solder Paste and Powders
      • Solder Research Kits
      • Spheres
      • Tape and Reel Packaging
      • Wire
      • Alloy Chart
    • Thermal Interface Materials
      • Heat-Spring®
      • NanoFoil®
      • Preforms
      • Ribbon and Foil
      • Other
      • Solder TIM
    • Thin-Film Materials
      • Featured Products
      • Sputtering Targets
      • Indium
      • Gallium
      • Others
  • Applications
    • Compounds
      • Batteries
      • Catalysts
      • Fiber Optics
      • LED MOCVD Precursors
      • Optical Lens
      • Reclaim and Recovery
    • Engineered Solder and Alloys
      • Connector Assembly
      • Cryogenic Seals
      • Die-Attach
      • Hermetic Sealing and Pass Throughs
      • IGBT
      • Medical Devices and Electronics
      • Thermal Management
    • LED
    • Low Temperature Alloys
    • Medical Devices and Electronics
    • PCB Assembly
      • Package-on-Package
      • Rework and Touch-Up
      • Solder Fortification®
      • Surface Mount
      • Thermal Management
      • Wave Solder
    • Semiconductor and Advanced Assembly
      • 2.5 and 3D Packages
      • Ball-Attach
      • Die-Attach
      • Flip-Chip
      • Pb-Free Including High Temperature Pb-Free
      • Shock Resistance Solutions
      • SnPb Including High Temperature High Pb
    • Thermal Management
      • Burn-in and Test
      • Concentrated Photovoltaic
      • IGBT
      • RF Power Devices
      • TIM1, TIM1.5, TIM2
    • Thin-Film
      • Thermal Evaporation
      • Plating
      • PV Sputtering Targets
      • Target Bonding
      • PVD Coating Materials
  • Contact Us

SUNTAB™ Specifications

Home » Products » Solar Assembly Materials » SUNTAB™ PV Ribbon » SUNTAB™ Specifications

  • SUNTAB™ Specifications
  • Related
    Technical Documents
  • Related
    Blog Posts

Base Copper (Rolled from round wire. CDA-110 (UNS-C110000). CDA-101 & CDA-102 also available.)

Purity 99.9%
Electrical Conductivity 101% IACS @ 68°F
Electrical Resistivity 1.72μΩ-cm
Coefficient of thermal expansion 9.40 x 10-6 per °F (68-212°F)

Common Dimensions (Custom dimensions available; just let us know what you need.)

  Tabbing Ribbon Bus Ribbon
Width +/- 76 µm 1.0 - 3.0 mm 5.0mm
Thickness +/- 8 µm .10 - .25 mm .10 - .30 mm

Alloys (Coating Thickness: 5-50µm per side.)

    Indalloy # Temperature (°C)
Tin/Lead 62Sn/36Pb/2Ag - 179° Eutectic
60Sn/40Pb 109 179°/138°
Lead-Free 96.5Sn/3.5Ag 121 221° Eutectic
100Sn 128 232°
Lead-Free / Low Temperature 58Bi/42Sn 281 138° Eutectic
57Bi/42Sn/1Ag 282 140°/139°
Low Temperature 46Bi/34Sn/20Pb 42 96° Eutectic

Mechanical Properties

Camber (mm/m): < 4.8
Available Yield Strengths
Rp0.2 (N/mm2):
Hard: < 140
Annealed: < 110
Soft: < 90
Super Soft: < 80
Elongation at fracture: > 25%

Packaging

Spool Specifications Diagram

Tabbing and bus ribbon is level-wound on ABS plastic spools (black for lead-containing and green for lead-free) in weights between 2.5kg to 4.54kg. Specialized packaging requirements, such as spool size and quantity per spool, can also be accommodated.

Spool D1 (mm) D2 (mm) D3 (mm) L1 (mm) L2 (mm)
P-5R 160 90 20 114 90
P-10S 152 102 15.90 122 102

Top SUNTAB™ Specifications Technical Documents

  • OnSpec® Solar Tabbing and Bus Ribbon (Letter) (A4)

    Product Data Sheet

SUNTAB™ PV Ribbon Specifications Technical Documents

Whitepapers

No whitepapers to display

Application Notes

No application notes to display

Product Data Sheets

OnSpec® Solar Tabbing and Bus Ribbon (Letter) (A4)

Material Safety Data Sheets

Solar Tabbing Ribbon

Solar Blog Posts

The Right Climate Stuff Research Team Hits the Mark

Tuesday, May 14, 2013 by Dr. Ron Lasky [view bio]

Folks, Many agree that the greatest technical achievement of human kind was landing a man on the moon and returning him safely to earth. (Just think about the fact that all of this was done with less computing power than your smartphone!).  Some of the folks involved in this effort  joined…

What Is Indium?

Friday, March 15, 2013 by Carol Gowans [view bio]

Being the Indium Corporation, we know what indium is, where it comes from, and how to use it.  But sometimes we forget that not everyone is as immersed in indium as we are. So what is indium?  Of course it is an element with an atomic number of 49, an atomic weight of 114.818amu, a relative…

Gallium Trichloride for Beginners

Tuesday, March 12, 2013 by Jim Hisert [view bio]

I’m not a chemist, so the first time I heard that we sell gallium trichloride (GaCl3) I was wondering “what the heck is this stuff, and what is it used for?” Years later, I’m still not a chemist, but I do understand what gallium trichloride is and what it’s used for. Gallium…

View All Blog Posts

#
Bill Jackson

This page is owned by:

Bill Jackson
Director, Solar Products
bjackson@indium.com

INDIUM CORPORATIONwww.indium.comaskus@indium.comPRC +86 (0)512 628 34900SINGAPORE +65 6 268 8678UK +44 (0) 1908 580400USA +1 315 853 4900

From One Engineer to Another®

Indium Corporation — ©1996–2013. All Rights Reserved. | Site Map

Related to SUNTAB™ Specifications

  • Liquid Tabbing Flux
  • Solder Paste
  • Sputtering Targets

Material Safety Data Sheets
Product Data Sheets
ISO and ITAR
Online Store
Tech Team

Connect with Indium

  • LinkedIn
  • Facebook
  • Twitter
  • YouTube
  • Blogger

+ Read our latest posts!

Americas

Utica, Chicago, Clinton
E-Mail: askus@indium.com
Phone: +1 315 853 4900

Asia/Pacific

Singapore, Cheongju
E-Mail: asiapac@indium.com
Phone: +65 6268 8678

China (中国网站)

Suzhou, Shenzhen, Liuzhou
E-Mail: china@indium.com
Phone: +86 (0)512 628 34900

Europe

Milton Keynes, Torino
E-Mail: europe@indium.com
Phone: +44 (0)1908 580400

Regional/Local Sales Support
Technical Service & Support

  • Home
  • Online Store
  • ISO and ITAR
  • Corporate
  • Tech Documents
  • MSDS
  • About Us
  • Jobs