Papers by Derrick Herron
Selection of Dip Transfer Fluxes and Solder Pastes for PoP Assembly
by Dr. Yan Liu, Pamela Fiacco, Derrick Herron, Dr. Ning-Cheng Lee
Consideration and selection of dip transfer fluxes and solder pastes for PoP assembly are described, based on process considerations. The crucial properties vital for successful dip transfer include homogeneity, open time on the flux/paste bed, volume and consistency of the dip transferred material, open time after the dip transfer before reflow, and solder joint formation. For each property, one or more practical, recommended test methods are described. Overall, this work should provide the assembly house with an easy way to select a flux or solder paste adequate for dip transfer of PoP assembly applications.
PoP, package-on-package, flux, solder paste, dip transfer, soldering, SMT
[Permanent Link to this Paper ]
Posted on 24 Jan 2011
Thermal Pad Design and Process for Voiding Control at QFN Assembly
by Derrick Herron, Dr. Yan Liu, Dr. Ning-Cheng Lee
Quad-flat no-leads (QFN) package designs are receiving more and more attention in the electronics industry. This package offers a number of benefits including (1) small size, such as a near die size footprint, thin profile, and light weight; (2) easy PCB trace routing due to the use of perimeter I/O pads; (3) reduced lead inductance; and (4) good thermal and electrical performance due to the adoption of exposed copper die-pad technology. These features make the QFN an ideal choice for many new applications where size, weight, electrical, and thermal properties are important. However, the adoption of QFN often runs into voiding issue at SMT assembly. Upon reflow, outgassing of solder paste flux at the large thermal pad has difficulty escaping and inevitably results in voiding. It is well known that the presence of voids will affect the mechanical properties of joints and deteriorate the strength, ductility, creep, and fatigue life. In addition, voids could also produce spot overheating, lessening the reliability of the joints. This is particularly a concern for QFN where the primary function of thermal pads is for heat dissipation. Thermal pad voiding control at QFN assembly is a major challenge due to the large coverage area, large number of thermal via, and low standoff. Both design and process were studied for minimizing and controlling the voiding. Eliminating the thermal via by plugging is most effective in reducing the voiding. For unplugged via situations, a full thermal pad is desired for a low number of via. For a large number of via, a divided thermal pad is preferred due to better venting capability. Placement of a thermal via at the perimeter prevents voiding caused by the via. A wider venting channel has a negligible effect on voiding and reduces joint continuity. For a divided thermal pad, the SMD system is more favorable than the NSMD system, with the latter suffering more voiding due to a thinner solder joint and possibly board outgassing. Performance of a divided thermal pad is dictated by venting accessibility, not by the shape. Voiding reduction increases with increasing venting accessibility, although the introduction of a channel area compromises the continuity of the solder joint. Reduced solder paste volume causes more voiding. Short profiles and long hot profiles are most promising in reducing the voiding. Voiding behavior of a QFN is similar to typical SMT voiding and increases with pad oxidation and further reflow.
voiding, thermal pad, solder, solder paste, SMT, flux, Apex 2011, QFN assembly
[Permanent Link to this Paper ]
Posted on 11 Apr 2011
Voiding Control for QFN Assembly
by Dr. Ning-Cheng Lee , Dr. Yan Liu, Derrick Herron
Quad Flat No Leads (QFN) package designs receive more and more attention in electronic industry nowadays. This package offers a number of benefits including (1) small size, such as a near die-sized footprint, thin profile, and light weight; (2) easy PCB trace routing due to the use of perimeter I/O pads; (3) reduced lead inductance; (4) easy PCB trace routing; and (5) good thermal and electrical performance due to the adoption of exposed copper die-pad technology. These features make the QFN an ideal choice for many new applications where size, weight, electrical, and thermal properties are important. However, adoption of QFN often runs into voiding issues at SMT assembly. Upon reflow, outgassing of solder paste flux at the large thermal pad has difficulty escaping and inevitably results in voiding. It is well known that the presence of voids will affect the mechanical properties of joints and deteriorate the strength, ductility, creep, and fatigue life. In addition, voids could also produce spot overheating, lessening the reliability of the joints. This is particularly a concern for QFN where the primary function of thermal pads is for heat dissipation. Thermal pad voiding control at QFN assembly is a major challenge due to the large coverage area, large number of via, and low standoff. Both design and process were studied for minimizing and controlling the voiding. Eliminating the via by plugging is most effective in reducing the voiding. For an open via situation, a full thermal pad is desired for a low number of via. For a large number of via, a divided thermal pad is preferred due to better venting capability. Placement of a via at the perimeter prevents voiding caused by via. A wider venting channel has a negligible effect on voiding and reduces joint continuity. For divided thermal pada, the SMD system is more favorable than the NSMD system, with the latter suffering more voiding due to a thinner solder joint and possibly board outgassing. Performance of a divided thermal pad is dictated by venting accessibility, not by the shape. Voiding reduction increases with increasing venting accessibility, although introduction of a channel area compromises the continuity of solder joint. Reduced solder paste volume causes more voiding. Short profiles and long hot profiles are most promising in reducing the voiding. Voiding behavior of a QFN is similar to typical SMT voiding and increases with pad oxidation and further reflow.
solder paste, reflow, SMT, solder, void
[Permanent Link to this Paper ]
Posted on 21 Feb 2011