  • Stress-Free Bonding of Large Linear Sputtering Targets for LCD Displays

    by A. Duckham, H.B. Parker, T.J. Acchione, M.A. Curran, J.E. Newson, N.G. Piegari, D.M. Lunking, E.L. Walters, D.B. Deger

    A process for bonding stress free, flat assemblies of late generation Liquid Crystal Displays (LCD) sputtering targets using reactive multilayer foil as a localized heat source has been developed. This paper will demonstrate the capability of bonding targets to backing plates of sizes up to those typical of Generation (Gen) 10 and on material combinations with widely divergent Coefficients of Thermal Expansion (CTE).

    sputtering target, NanoFoil, NanoBond, LCD, target bonding