  • Engineering Solder Paste Performance Via Controlled Stress Rheology Analysis

    by Dr. Anu Maria, K. P. Rangan, Rajkumar B. Raj, Dr. Ning-Cheng Lee, Dr. Xiaohua Bao

    Rheology of a solder paste has a significant effect on its stencil printing, tack, and slump performance. This paper describes a series of tests designed to investigate the rheological properties of a suite of solder pastes and fluxes, and the correlation with the solder paste performance prior to reflow. Data indicate that 1) print defect is proportional to the compliance (J1 and J2) and inversely proportional to the elastic properties (G’/G’’ and Recovery) and meta-rigidity (Yield Stress); 2) slump resistance is proportional to elastic properties (Recovery), solid characteristics (Stress [G’=G’’]), and rigidity ( êG* ê); 3) high elastic properties (Recovery), low compliance (J1 and J2), and low solid characteristics (Stress [G’=G’’]) are required in order to achieve high tack value. Good correlation between fluxes and solder pastes are observed for Yield Stress and Recovery only, suggesting those two properties are primarily dictated by fluxes.

    lead-free, pb-free, viscosity, flux, tack, slump, print, rheology, solder paste, soldering, solder