  • Effect of Nano-Coated Stencil on 01005 Printing

    by S. Manian Ramkumar Ph.D., Rita Mohanty Ph.D., CEMA, Chris Anglin, Toshitake Oda

    The demand for product miniaturization, especially in the handheld device area, continues to challenge board assembly industry. The desire to incorporate more functionality while making the product smaller continues to push board design to its limit. It is not uncommon to find boards with castle like components right next to miniature components. This type of board poses special challenge to the board assemblers as it requires wide range of paste volume to satisfy both small and large components. One way to address the printing challenge is to use creative stencil design to meet the solder paste requirement for both large and small components. Example of stencil design includes step stencil, dual printing, over size aperture, etc. Stencil printing process at its most basic level involves pushing solder paste through a stencil (with various size apertures) by a squeegee blade. As the squeegee blade and the stencil are in constant contact with the paste during the printing process, their surface characteristics play an important role in the printing process. The most important attribute of a stencil is its release characteristic. In other word, how well the paste releases from the aperture. The paste release in turn depends on the surface characteristics of the aperture wall and stencil foil surface. Recent introduction of a new technology, Nano-coating for both stencil and squeegee blades, has drawn the attention of many researchers. As the name implies, Nano-coated stencils and blades are made by conventional method such as laser cut or Electoform then coated with nano functional material to alter the surface characteristics. This study will evaluate nano-coated stencils for passive component printing including 01005. Various print experiments will be conducted using different stencil technology, stencil thicknesses, aperture size, aperture orientation, aperture shapes, and selected paste type with optimal print parameters, to understand the effect of chosen factors on the print quality. Print quality will be determined by visual inspection and 3D measurement of the paste deposit to understand the volume transfer efficiency.

    Apex 2011, solder paste, transfer efficiency, area ratio, stencil technology, broadband printing, nano-coated stencil