Engineering Drawing / Specifications for Pure Indium Preforms
Missing dimensions can be resolved, but checking for this before sending the drawing can eliminate the time needed to solve the issue. Thorough drawin...
Missing dimensions can be resolved, but checking for this before sending the drawing can eliminate the time needed to solve the issue. Thorough drawin...
Indium metal preforms need specialized packaging to ensure they arrive at your facility safetly and securely. Let us help you choose just the right pa...
Jim Hisert enlists Meagan Sloan, Technical Support Engineer to recommend a flux for his indium preform application. ...
Great news! Liquid metal for prototyping, low-volume applications, or even overclocking is more accessible that ever before....
Durafuse® LT gives us even more options for low-temperature solder reflow, but thankfully just using consistent terminology can go a long way...
Durafuse® LT is a low-temperature solder with two different liquidus temperatures - one lower and one higher than the the peak reflow tempera...
Low temperature solder Durafuse® LT's drop-shock test is two orders of magnitude better than the drop shock test of a BiSnAg alloy....
Since pure indium preforms are so soft, making thousands of parts requires different processing and packaging methods than manufacturing jus...
New Durafuse® LT is a novel mixed alloy system designed to combine low temperature solder reflow with drop-shock performance similar to or be...
We have all ordered something in the wrong size - it’s frustrating! Today we discuss specifying the dimensions for pure indium preforms....
Indium is commonly available from 99.9% to 99.9999% purity, although 99.995-99.999% is recommended most often for vacuum, hermetic, and cryogenic seal...