Why Not Subscribe to the Indium TIM Blog
Enjoy reading my postings about my experience with cooling......
Enjoy reading my postings about my experience with cooling......
Where would we be without advancement? Sure, some of our modern world......
Pure indium or indium alloys are used to form hermetic seals that also conduct heat. Indium washers......
At what point in new product development does the solder get updated with the rest of......
Have you seen the statement on Indium’s product data sheet for liquid metals that says: “Care should be taken in reheating the alloy in th...
Ok, so it happened again. Another urgent request was brought to me for action. This time it was a customer who had performed a Red Dye Penetration......
Calculating the thermal conductivity of an alloy is not done by taking an average (or weighted average) of its elemental constituents. When two metals...
Alan Fairbairn Guest Blogger European Business Development Manager Engineered Solders Materials I hope I can bring a European flavour to Engine...
Due to the limitations of flux, there is bottom end temperature where traditional solder/flux bonding ends. The lowest temperature I have experienced ...
The most common metal thermal interface materials are made from indium alloys which melt between 100C to 200C. Some power devices I have come across d...