Solder Paste for Low Temperature and Pb-Free Applications
There are a lot of parameters to consider when choosing the right solder for your application: 1) The operational temperature of the final device p st...
There are a lot of parameters to consider when choosing the right solder for your application: 1) The operational temperature of the final device p st...
Folks, There is a lot of interest in cleaning PCBs that have been assembled with no-clean solder pastes. Recently I discussed the topic with my ...
Maria Durham, Indium’s new Technical Specialist in Semiconductor and Advanced Assembly Materials, has been doing some research on indium lead (I...
Reducing the surface oxides of Nitinol is just the first step in getting a good solder joint with this versatile medical assembly material. Next you h...
Folks, Patty is getting ready for her meeting on “Copy Exactly” with Mike Madigan….... It was after 6:30 PM and Patty was just arri...
I recently had a chance to catch up with a friend and colleague, Jasbir Bath. If you’ve spent time in the electronics assembly industry you have...
Readers have asked how to visually assess a tabbing ribbon interconnection after a bond test. This image is a cell that has been bond tested after sol...
Folks, A reader writes: My company makes an electronic product that requires a 40 year shelf life. We assemble with tin-lead solder on FR-4 PWBs....
After the report by Isofoton regarding reliability testing of Bi-based alloys for tabbing ribbon, the world learned that Bi-based alloys could survive...
Two categories of solder are available to choose from when the in-service environment for a device reaches above 125°C either in continuous operat...
在SMT中,底部填充剂(underfill) 常常被用在BGA/QPN 的组装...
Indium and indium-containing alloys see wide use in a multitude of soldering applications. Indium has many attractive properties such as remaining duc...