Response-to-Pause: A Critical Solder Paste Parameter
Folks, Solder paste is arguably the most highly engineered material in electronic assembly. It has many properties that must be favorable for its good...
Folks, Solder paste is arguably the most highly engineered material in electronic assembly. It has many properties that must be favorable for its good...
Folks, I recently developed some Excel®-based software to help those who are planning to take the SMTA certification exam to practice. Software to...
There is a big difference between a reflow profile and the oven settings. A cooking analogy can help explain the difference....
A paper presented at SMTAI 2016 on reducing voids in bottom-terminated components......
Folks, Everyday, we are exposed to the results of surveys and polls. A typical example might be that President Obama is leading Mitt Romney in a...
Solder starvation is a serious electronics assembly issue – with a very simple solution. Solder starvation occurs when adequate volumes of solde...