Optimize the Zero Stress Point
An important quote from Eliminating Bond Stresses of Sputtering Targets at Operating Temperatures is: “This suggests that a target bonded at one...
An important quote from Eliminating Bond Stresses of Sputtering Targets at Operating Temperatures is: “This suggests that a target bonded at one...
We have observed that the temperature at which two materials are bonded will set the base temperature that any subsequent CTE is measured from. T...