Indium Corporation to Feature Ultra-Low Voiding Indium10.1HF Solder Paste at Productronica China 2018
February 15, 2018
Indium Corporation will feature its new ultra-low voiding Indium10.1HF Solder Paste—which helps customers Avoid the Void®—at Productronica China 2018, March 14-16, 2018, in Shanghai.
Indium10.1HF is an air reflow, no-clean, halogen-free, Pb-free solder paste specifically formulated to achieve ultra-low voiding, especially in bottom termination component (BTC) assemblies.
Indium10.1HF has a flux chemistry engineered to improve reliability with:
- High ECM performance under low standoff components, RF shields without proper ventilation, and components in low-clearance cavities
- Solder beading minimization
- Very low bridging, slump, and solder balling
- Excellent wetting to a variety of common fresh and aged metallizations and surface finishes
- High print transfer efficiency with low variation
Indium10.1HF is compatible with lead-free alloys such as SnAgCu, SnAg, and other alloy systems favored by the electronics industry. This solder paste is halogen-free per IEC 61249-2-21, test method EN 14582.
For more information about Indium Corporation’s low-voiding solder pastes, visit www.indium.com/avoidthevoid or see Indium Corporation at booth E2.2330.
For more information about Indium Corporation, visit www.indium.com or email abrown@indium.com. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.