Indium Corporation announces the release of PoP Flux 89LV-P, a bright pink-colored, no-clean, thixotropic flux that helps engineers to Avoid the Void™ by greatly improving visual inspection to minimize voiding and other defects in package-on-package applications.
Designed for package-on-package assembly applications, PoP Flux 89LV-P contains a pink dye that is highly visible to the naked eye but is not picked up by automated vision systems. Therefore, PoP Flux 89LV-P does not cause false rejects on equipment that cannot decipher grayscale differences.
“You can practically see our new pink flux from outer space,” said Christopher Nash, PCBA New Product Development Manager. “Of course, that is an exaggeration, but it is very easy to visually inspect. This allows quick confirmation that the flux is present while setting up the process or performing visual process verification.”
In addition to its visual properties, PoP Flux 89LV-P has a unique activator system that provides enhanced solderability onto all common metallizations.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, thermal management, and solar markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, Indium has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
For more information about Indium Corporation, visit www.indium.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.