We are frequently asked if it is possible to solder to aluminum. The answer is yes, if the following guidelines are followed: FLUXES: Becau...
We are frequently asked if it is possible to solder to aluminum. The answer is yes, if the following guidelines are followed: FLUXES: Becau...
After the report by Isofoton regarding reliability testing of Bi-based alloys for tabbing ribbon, the world learned that Bi-based alloys could survive...
Folks, I’m taking a few moments from Wassail Weekend , held annually in my village, Woodstock VT, “The prettiest small town in Americ...
Tombstoning (also known as the Manhattan effect, drawbridge effect, or Stonehenge effect) is described (in the simplest, and most common, sense) as oc...
Here is a list of tricks to help you overcome the issues that can arise while hand soldering silicon-based solar cells (and other applications as well...
Solder paste is comprised of powdered solder alloy suspended in a flux vehicle. There is a group of flux ingredients that is generically identified as...
Folks, The Guadalajara (GDL), MX Chapter of the SMTA held their first meeting on November 9 and 10 at CETI in GDL. Approximately 70 engineers from......
Following on from our discussions of last time... As you will recall from the previous post on this topic, My friend and colleague Chris Nash and I w...
My friend and colleague Chris Nash and I were recently discussing some puzzling results for low dip height found during testing of package-on-pac...
最近越来越多的客户都在询问Indium Flux #2,其中有...
Hi there! I am excited, this is my first blog post -ever. I am excited that it is a technical blog of Indium Corporation. My story is very ...
Solder powder particle size and shape impacts the functionality of solder paste in many ways: printing/dispensing/dipping; solderballing; graping; voi...