Indium Corporation manufactures 60 different alloys that contain indium, in addition to over 150 other non-indium-bearing alloys, such as SAC and...
Indium Corporation manufactures 60 different alloys that contain indium, in addition to over 150 other non-indium-bearing alloys, such as SAC and...
Today I was sent an article that involves TWO of my favorite elements, indium and gallium which, when combined with tin, creates an alloy that is...
Gallium has a melting point of ~30°C (86°F), which makes the physical state of the metal as predictable as the shipping temperatures it endure...
Today we discuss the technology behind the paper: “Extreme Toughening of Soft Materials with Liquid Metal” with Dr. Navid Kazem....
What does the future bring for self-healing circuits? Electrical self-healing is important, but what about mechanial self-healing?...
What are some real-world applications for stretchable electronics made of gallium and indium - both near-term and long-term?...
Self-healing electronics seems moer like magic than science. The secret to this magic is the unique material architecture....
Jim Hisert discusses the composite material that is electrically insulating until it is patterned, at which point it becomes conductive....
Jim Hisert discusses the future of self-healing electronics with Eric Markvicka of Carnegie Mellon University....
GaIn alloys are non-toxic and not highly reactive, making them ideal for use in many liquid metal applications....
There were many positive changes to the SVC show for 2018 . Here is a little of what you missed if you weren't there....
Jim Hisert, Indium Applications Manager, and Phil Zarrow take a look a liquid metal and its current and potential applications. ...