The Importance of Oxygen Barrier in Solder Pastes
Folks, Pity the solder scientists of the late 1970s and early 1980s. SMT was an emerging technology and the world wanted to buy solder paste.&nb...
Folks, Pity the solder scientists of the late 1970s and early 1980s. SMT was an emerging technology and the world wanted to buy solder paste.&nb...
Indium metal powder is mixed with flux for application by dispensing or printing equipment. This mixture is referred to as solder paste. Lucky fo...
Interesting question from a Chinese die-attach customer this week asking about volume resistivity of solder. My friend, Eric Bastow, suggested that In...
People use indium in many forms – to create many different products. Certain forms fit various applications. Here are some of the many forms of ...
Eric is a Senior Tech Support Engineer, and he’s one of the guys I turn to when I receive really tricky questions. He has a great deal of experi...
While not directly part of Indium Corporation’s Technical Service department, Maria is technology driven and works with our customers to help se...
Many people try to determine the volume of solder paste that they will use on a given circuit board or during a full production run. Calculating...
The 46th International Symposium on Microelectronics will be held in Orlando, Florida, September 30th through October 3rd, 2013. I will be attending b...
Today we focus on Derrick Herron – one of the newest members of Indium Corporation’s Technical Services team. While new to tech servi...
Solder seems pretty simple, and, honestly, it doesn’t always need to be overly technical. But, many SMT, semiconductor, thermal management, and ...
NanoFoil® is especially well-suited for bonding LED packages. Here are some characteristics of the NanoBond® Process that fit high v...
We have all seen the action movies where the hero drops in at the last minute to save the day against insurmountable odds. NanoFoil® is like...