As previously posted, Indiums Table of Specialty Alloys҂and solderscontains hundreds of solder alloys and for each of them, we have listed melting temperatures. The method by which these were calculated is a repeatable one using a piece of equipment called a Differential Scanning Calorimeter.
In this method, a small sample of the solder alloy is input into the system and slowly heated until the solder alloy melts.Throughout the reading, a graph is created, from which the solidus and liquidus temperatures are interpreted.
The graph appears as a steady baseline, and at the melting point of the solder alloy, a peak is generated (See Image).At the point where the peak first deviates from the baseline, the solder alloy has begun to melt and this is the solidus point.At the point where the deviation returns to the baseline, the solder alloy is completely molten and this is theliquidus point. The entire deviation period is defined as a phase change period.
The tolerance of the scan is related to the scan rate.The slower the scan, the more accurate the reading.The tolerance on a typical reading is +/- 3:C.
Nếu bạn có thắc mắc về nhiệt độ nóng chảy của bất kỳ hợp kim hàn nào của chúng tôi hoặc hợp kim hàn mà bạn mua từ chúng tôi, chúng tôi sẽ rất vui lòng chia sẻ các chỉ số nhiệt lượng kế quét vi sai để bạn có thể tự giải thích.