Packaging NanoFoil® Preforms

NanoFoil® can be packaged in tape & reel, bulk containers, or waffle packages. Here are the main advantages of each type of packaging:

  • Tape & Reel: great choice for high-volume automated pick & place equipment
  • Waffle Pack: perfect for hand placement or low-volume automated placement machines
  • Bulk: most economical way to order

Packaging NanoFoil® is actually a lot like packaging standard solder preforms. (Here is a complete list of our packaging options for preforms.)