Indium Corporation has announced a new jetting solder paste in its line of PicoShot products. PicoShot WS-5M is designed for customers needing an SnPb solder paste for their Mycronic MY-series jet printers.
PicoShot WS-5M is a water-soluble, halogen-free paste developed as a result of a close, collaborative relationship with Mycronic for their MY 600/700 jetting systems. This product has been beta-tested at customer sites, showing proven performance on customer lines.
PicoShot WS-5M has been extensively tested to provide exceptional jetting performance. It delivers:
- Smallest dot volume among pastes in its class: 6.5nl/dot, 350m diameter
- Precision deposit (x,y targeting)
- Long usage (syringe life) >8 hours
- Minimal statellites
PicoShot WS-5M is a water-soluble, halogen-free solder paste approved after joint Indium/Mycronic technical development with Mycronic’s MY 600/700 jetting systems. PicoShot can be used in applications, such as jetting into cavities and uneven/warped substrates, high-mix/low-volume stencil replacement, CSP/microBGA solder attach, military and aerospace jetting applications, system-in-package (SiP), camera module assembly where an overmolding step is required, and shield-attach and secondary processing.
Utilizing a Type 5 solder powder and an SnPb alloy, this material is inherently chemically compatible with Indium Corporation’s Indium6.6HF-HD Solder Paste. PicoShot WS-5M’s unique oxidation barrier promotes complete powder coalescence during reflow to eliminate graping and similar reflow issues.
PicoShot WS-5M jetting solder paste is the second material to come out of Indium Corporation’s new partnership with Mycronic, a global leader in dispensing and jet printing equipment.
To learn more about Indium Corporation’s jetting pastes, visit https://www.indium.com/products/solders/solder-paste/#jetting-and-microdispensing.
Sobre a Indium Corporation
A Indium Corporation é um dos principais refinadores, fundidores, fabricantes e fornecedores de materiais para os mercados globais de eletrónica, semicondutores, película fina e gestão térmica. Os produtos incluem soldas e fluxos; brasagens; materiais de interface térmica; alvos de pulverização; metais e compostos inorgânicos de índio, gálio, germânio e estanho; e NanoFoil. Fundada em 1934, a empresa tem apoio técnico global e fábricas localizadas na China, Alemanha, Índia, Malásia, Singapura, Coreia do Sul, Reino Unido e EUA.
Para mais informações sobre a Indium Corporation, visiteindiumstg.wpenginepowered.comou envie um e-mail paraJingya Huang. Também pode seguir os nossos especialistas, «From One Engineer To Another»(#FOETA), emwww.linkedin.com/company/indium-corporation/ou@IndiumCorp.