Durafuse, Indium Corporations award-winning mixed-alloy technology, will be the focus of a virtual presentation by Dr. HongWen Zhang for the Institution of Engineers, Malaysia at 8 a.m. New York/9 p.m. Malaysia on Thursday, Feb. 24.
In The Basic Challenges of Solder Materials and our Solutions with Durafuse Technology, Dr. Zhang will discuss the basic shortcomings of traditional solder materials and will examine the ability of Indium Corporations Durafuse technology to provide a solution to these challenges. Dr. Zhang will highlight the benefits of Durafuse LT, a patent-pending, innovative low-temperature mixed-alloy technology that offers enhanced reliability with drop shock performance two orders of magnitude better than Bi-containing solders. He will also discuss Durafuse HT, a new product designed as a drop-in solution to replace and outperform the traditional high-lead solders in die-attach and clip-bond applications.
Dr. Zhang is manager of the Alloy Group within Indium Corporations Research & Development Department. His focus is on the development of lead-free solder materials and the associated technologies for high-reliability applications. He and Dr. Ning-Cheng Lee invented the mixed-alloy solder technique to combine the merits of constituents to improve wetting, reduce processing temperatures, modify the bonding interface, and control the joints morphology, thus improving the reliability. On the basis of this technique, the Durafuse LT, BiAgX, and Durafuse HT solder systems were invented to meet the market need. He has published more than 20 papers and journal articles. Dr. Zhang received his Ph.D. in materials science and engineering, as well as a masters degree in mechanical engineering from Michigan Technological University. He holds a Lean Six Sigma Green Belt and is a certified IPC specialist for A-600 and IPC-A-610D and a certified SMT Process Engineer.
Sobre a Indium Corporation
A Indium Corporation é um dos principais refinadores, fundidores, fabricantes e fornecedores de materiais para os mercados globais de eletrónica, semicondutores, película fina e gestão térmica. Os produtos incluem soldas e fluxos; brasagens; materiais de interface térmica; alvos de pulverização; metais e compostos inorgânicos de índio, gálio, germânio e estanho; e NanoFoil. Fundada em 1934, a empresa tem apoio técnico global e fábricas localizadas na China, Alemanha, Índia, Malásia, Singapura, Coreia do Sul, Reino Unido e EUA.
Para mais informações sobre a Indium Corporation, visiteindiumstg.wpenginepowered.comou envie um e-mail paraJingya Huang. Também pode seguir os nossos especialistas, «From One Engineer To Another»(#FOETA), emwww.linkedin.com/company/indium-corporation/ou@IndiumCorp.
About Institution of Engineers, Malaysia
The Institution of Engineers, Malaysia was established in 1959 and its primary function is to promote and advance the science and profession of engineering in any or all of its disciplines and to facilitate the exchange of information and ideas related to engineering.