Indium Corporation Introduces New Ball-Attach and Flip-Chip Flux

Indium Corporation has expanded its flux portfolio with a robust flux designed to provide a simple solution to complicated applications, especially those with a single cleaning step for both BGA ball-attach and flip-chip processes.

WS-446HF is a water-soluble, halogen-free, flip-chip dipping flux with an activator system powerful enough to promote good wetting on the most demanding surfaces—including solder-on-pad (SoP), Cu-OSP, ENIG, embedded trace substrates (ETS), and flip-chip on leadframe applications.

WS-446HF:

  • Includes a chemistry that eliminates dendrite issues, especially critical for fine-pitch flip-chip applications
  • Provides tackiness suitable for holding solder spheres and large die in place during assembly, eliminating missing balls and reducing die tilt and non-wet-opens due to warpage
  • Delivers consistent pin transfer, printing, and dipping performance, ensuring consistent joint quality and improving production yields
  • Eliminates the need for multiple fluxing steps, enabling a single-step ball-attach process and eliminating the warpage-inducing effects of prefluxing
  • Has good cleanability with room temperature DI water, avoiding the formation of white residue

A Indium Corporation é um dos principais fabricantes e fornecedores de materiais para os mercados globais de eletrónica, semicondutores, película fina e gestão térmica. Os produtos incluem soldas e fluxos; brasagens; materiais de interface térmica; alvos de pulverização; metais e compostos inorgânicos de índio, gálio, germânio e estanho; e NanoFoil®. Fundada em 1934, a empresa tem apoio técnico global e fábricas localizadas na China, Índia, Malásia, Singapura, Coreia do Sul, Reino Unido e EUA.