Indium is a soft and malleable metal that stretches with the metal it’s soldered to. This makes it the perfect solder for joining two metals in order to avoid coefficient of thermal expansion (CTE) mismatch.
CTE mismatch occurs when solder joints containing two different metals expand at different rates. This stress on the solder joint can cause it to crack upon cooling, resulting in the failure of the device.
For more information on indium metal, visit indiumstg.wpenginepowered.com/indium49.
Indium Corporation là nhà sản xuất và cung cấp vật liệu hàng đầu cho các thị trường điện tử, bán dẫn, màng mỏng và quản lý nhiệt toàn cầu. Các sản phẩm bao gồm chất hàn và chất trợ dung; hàn đồng; vật liệu giao diện nhiệt; mục tiêu phun; kim loại indium, gali, germani và thiếc và các hợp chất vô cơ; và NanoFoil ® . Được thành lập vào năm 1934, công ty có hỗ trợ kỹ thuật toàn cầu và các nhà máy đặt tại Trung Quốc, Malaysia, Singapore, Hàn Quốc, Vương quốc Anh và Hoa Kỳ.
Để biết thêm thông tin về Indium Corporation, vui lòng truy cậpindiumstg.wpenginepowered.comhoặc gửi emailđến [email protected]. Quý vị cũng có thể theo dõi các chuyên gia của chúng tôi, From One Engineer ToAnother®(#FOETA), tạiwww.facebook.com/indiumhoặc@IndiumCorp.