Indium Corporation Introduces Indalloy291 Supplemental Bar Alloys

Indium Corporation announces that it is now offering supplemental bar alloys for Indalloy291 wave solder pots designed to maintain recommended solder pot specifications. 

The supplemental bar and bar chips are added to Indalloy291-containing solder pots that have fallen below or have elevated above the recommended specifications. This can be determined by solder analysis performed by Indium Corporation. 

During wave soldering, when the molten solder contacts the air and manufacturing environment, a chunky layer of metal collects on the smooth surface of the molten soldersolder dross. Indium Corporation’s Dross Reduction Bar aids in the reduction of this solder dross build-up within Indalloy291 solder pots. By reducing dross formation, the Dross Reduction Bar also reduces the amount of solderable metal lost in the solder pot, providing the user a considerable cost-savings over time.

If instead during wave soldering the molten solder contacts a copper-containing PCB, such as an OSP board, the copper from the board can be pulled into the solder wave, increasing the solder pot’s copper content to an undesirable level. As copper levels gradually rise to become out-of-spec within an Indalloy291 solder pot, adverse effects to wetting performance and solder joint aesthetics can become more perceptible. Indium Corporation’s Replenisher Bar is used to bring the copper levels back within the recommended solder pot specifications.

Indium Corporation also offers a solder and solder dross recycle program to complete the usage cycle for bar solder. Up to 50% of bar solder used in wave soldering will be converted to dross, which still contains mostly usable metal. Indium Corporation can recycle these materials and return the metal value to you as a credit, or convert them to a usable bar for a fee. During an alloy switchover, use Indium Corporation’s recycling service to reclaim value on the pot dump and leftover bar. For more information about Indium Corporation’s solder and solder dross recycle program, please send an email to [email protected].

For more information, visit https://www.indium.com/products/solders/bar-solder/ or contact Robert McKerrow, Senior Product Specialist Flux-Cored Wire, Wave Solder Flux, and Bar Solder, here.

Giới thiệu về Indium Corporation

Indium Corporation là một nhà tinh chế vật liệu, nhà luyện kim, nhà sản xuất và nhà cung cấp hàng đầu cho các thị trường điện tử, bán dẫn, màng mỏng và quản lý nhiệt toàn cầu. Các sản phẩm bao gồm chất hàn và chất trợ dung; chất hàn; vật liệu giao diện nhiệt; mục tiêu phun; kim loại indium, gali, germani và thiếc và các hợp chất vô cơ; và NanoFoil . Được thành lập vào năm 1934, công ty có hỗ trợ kỹ thuật toàn cầu và các nhà máy đặt tại Trung Quốc, Đức, Ấn Độ, Malaysia, Singapore, Hàn Quốc, Vương quốc Anh và Hoa Kỳ

Để biết thêm thông tin về Indium Corporation, vui lòng truy cậpindiumstg.wpenginepowered.comhoặc gửi email choJingya Huang. Bạn cũng có thể theo dõi các chuyên gia của chúng tôi, From One Engineer To Another(#FOETA), tạiwww.linkedin.com/company/indium-corporation/hoặc@IndiumCorp.