Indium Corporation Launches New Indium Oxide

Indium Corporation has released IndiOx™ (In2O3) for use in the manufacture of ITO sputtering targets for thin-film coating. IndiOx™ (In2O3) is a stable ceramic-like material that is insoluble in water and volatizes at 850°C. 

When doped with tin oxide, IndiOx™ forms ITO, the material of choice to form transparent conductive oxide (TCO) layers in flat-panel displays and touch sensors for mobile devices. The ITO layer is deposited onto glass from a sputtering target that is manufactured from the ITO powder by sintering.   

Other uses for IndiOx™ include glass coloring, gassing suppression in alkaline batteries, and as an anti-arcing additive in high current electrical switches and contactors.

IndiOx™ is available in three powder types:

  • Type A – Crystalline: particle size distribution D10–D90 ranges from 0.8–38μm. 
  • Type B – Fine: particle size distribution D10–D90 ranges from 0.5–6μm. 
  • Type T – Target Grade: particle size distribution D10–D90 ranges from 0.1–7.5μm. The primary particle size is about 100nm.

For more information about Indium Corporation’s suite of compound materials, visit indiumstg.wpenginepowered.com/indiox.

Indium Corporation là nhà sản xuất và cung cấp vật liệu hàng đầu cho các thị trường điện tử, bán dẫn, màng mỏng và quản lý nhiệt toàn cầu. Các sản phẩm bao gồm chất hàn và chất trợ dung; hàn đồng; vật liệu giao diện nhiệt; mục tiêu phun; kim loại indium, gali, germani và thiếc và các hợp chất vô cơ; và NanoFoil ® . Được thành lập vào năm 1934, công ty có hỗ trợ kỹ thuật toàn cầu và các nhà máy đặt tại Trung Quốc, Ấn Độ, Malaysia, Singapore, Hàn Quốc, Vương quốc Anh và Hoa Kỳ.

Để biết thêm thông tin về Indium Corporation, vui lòng truy cậpindiumstg.wpenginepowered.comhoặc gửi emailđến [email protected]. Quý vị cũng có thể theo dõi các chuyên gia của chúng tôi, From One Engineer ToAnother®(#FOETA), tạiwww.facebook.com/indiumhoặc@IndiumCorp.