Indium Corporation has released a new halogen-free, no-clean ROL0 flux specifically developed for PCB assembly hand soldering and rework applications.
TACFlux® 020B-RC passes SIR testing in the unreflowed state. Oftentimes during hand soldering and rework, the flux may not be heated properly due to spot heating methods, thus the flux is not adequately activated. TACFlux® 020B-RC is designed to solve this problem and avoid reliability concerns such as dendritic growth over time.
TACFlux® 020B-RC joins Indium Corporation's versatile offering of specialty fluxes designed to provide solutions for current and evolving industry challenges. Benefits of TACFlux® 020B-RC include:
- Passes J-STD-004B SIR testing in the unreflowed state
- Halogen-free per IEC 61249-2-21 test method EN14582
- Outstanding wetting performance on difficult to solder metallizations
- Designed for no-clean applications, but flux can be removed using a commercially-available flux-cleaner
For more information about TACFlux® 020B-RC, visit indiumstg.wpenginepowered.com/flux-and-epoxy/tacky-flux.
Indium Corporation là nhà sản xuất và cung cấp vật liệu hàng đầu cho các thị trường điện tử, bán dẫn, màng mỏng và quản lý nhiệt toàn cầu. Các sản phẩm bao gồm chất hàn và chất trợ dung; hàn đồng; vật liệu giao diện nhiệt; mục tiêu phun; kim loại indium, gali, germani và thiếc và các hợp chất vô cơ; và NanoFoil ® . Được thành lập vào năm 1934, công ty có hỗ trợ kỹ thuật toàn cầu và các nhà máy đặt tại Trung Quốc, Malaysia, Singapore, Hàn Quốc, Vương quốc Anh và Hoa Kỳ.