Environmental and legislative concerns are driving consumers away from products using solders that contain lead (Pb), including solders used in die-attach applications for analog semiconductor assembly. Indium Corporation’s BiAgX® solder paste technology is a high-melting, lead-free (Pb-free) solder paste technology that serves as a drop-in replacement for the high-Pb solders used in many high-reliability die-attach and electronics assembly applications.
BiAgX can survive junction temperatures and high-temperature environments in excess of 175°C with little degradation of the mechanical structure or other properties.
“BiAgX is the only low-cost, customer-proven, lead-free replacement solder paste that is able to survive J-STD-020 MSL reflow profiles (up to 260°C) in the final solder joint,” said Indium Corporation’s Andy C. Mackie, PhD, MSc, senior product manager for semiconductor and advanced assembly materials. “BiAgX has been qualified by customers at moisture sensitivity level (MSL) 3 up to 1 per IPC/JEDEC Standard J-STD020. Customers are also ramping production to meet their customers’ needs for a completely lead-free final assembly.”
BiAgX is suited for small, low-voltage QFN packages that are used in portable electronics (smartphones/tablets), automotive electronics, and industrial applications. It requires minimal process adjustments and no capital expenditures for customers converting from a standard high Pb-containing solder paste-based process. It is both Pb-free and Sb-free (lead and antimony) and does not contain costly specialty materials, such as nanosilver or sintering aids.
BiAgX reflows, solders, wets, and solidifies just like any other solder paste, and is available in both dispense and printing forms. Flux residues are easily cleanable with standard cleaning chemistries and processes.
For more information about BiAgX, including technical papers and other technical information, visit indiumstg.wpenginepowered.com/BiAgX.
Indium Corporation là nhà sản xuất và cung cấp vật liệu hàng đầu cho các thị trường điện tử, bán dẫn, năng lượng mặt trời, màng mỏng và quản lý nhiệt toàn cầu. Các sản phẩm bao gồm chất hàn và chất trợ dung; hàn đồng; vật liệu giao diện nhiệt; mục tiêu phun; kim loại indium, gali, germani và thiếc và các hợp chất vô cơ; và NanoFoil ® . Được thành lập vào năm 1934, Indium có hỗ trợ kỹ thuật toàn cầu và các nhà máy đặt tại Trung Quốc, Malaysia, Singapore, Hàn Quốc, Vương quốc Anh và Hoa Kỳ.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.