Indium Corporation is a leading gold solder innovator for high-temperature and high-reliability applications, such as die-attach and hermetic sealing in medical, aerospace, optoelectronics, automotive, and many other industries.
Gold-based alloys offer strong joints, excellent corrosion and oxidation resistance, and good thermal and electrical transfer at the joint. Our gold solder portfolio includes wire, paste, preforms, and ribbon. They are manufactured with cutting-edge technology to ensure quality as well as push the boundaries of precision.
Higher yields and cost per unit make gold a viable option for many applications, even though the initial cost is more than alternative solders. A low oxygen atmosphere may be required if the application is flux free. In some instances, pressure is required to promote strong, void-free reflow on horizontal services.
Attributes
Gold solder is known for strong bond strength, excellent corrosion and oxidation resistance, and reliable thermal and electrical transfer at the braze joint.
Processing Options
Choose from proven processing methods, including: vacuum soldering, die-attach, reflow, laser soldering, vapor phase reflow, and manual soldering.
Features
We offer more than 320 alloy solutions capable of withstanding temperatures up to 1,100°C. Innovative lead-free alternatives—including gold solders, sintering, preforms, and advanced alloy technologies integrated with new flux systems—are also part of our ongoing development efforts.
>280°C
High melting point compatible with subsequent reflow processes.
Critical Applications
Automotive, RF infrastructure, medical, laser, military, and aerospace applications.
Pb-free
Lead-free and RoHS compliant.
#1 in Reliability
Highest tensile strength of any solder.
Gold-Based Alloys
Indium Corporation offers a broad range of gold-based alloy solutions with melting temperatures up to 1,064°C:
Alloy Name
Composition
Melting Point
Indalloy®182
80Au20Sn
280°C Eutectic
Indalloy®200
100Au
1,064°C Eutectic
Indalloy®178
82Au18In
Solidus 451°C / Liquidus 485°C
Indalloy®184
96.8Au3.2Si
363°C Eutectic
Indalloy®183
88Au12Ge
356°C Eutectic
Indalloy®270
75Au25Sn
Solidus 278°C / Liquidus 332°C
Indalloy®269
78Au22Sn
Solidus 278°C / Liquidus 301°C
Indalloy®271
79Au21Sn
Solidus 278°C / Liquidus 289°C
Gold Solder Products
With years of experience in the industry, we have built a strong foundation of knowledge and expertise in solving manufacturing challenges. We provide a wide array of alloys and flux choices, leveraging our technical proficiency to act as a strategic ally for each client, ensuring the delivery of exceptional results and performance.
Indium Corporation is a leading gold solder innovator for high-temperature, high-reliability, and critical applications such as die-attach and hermetic sealing in:
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!
Folks, Let’s check in on Rob, while Patty is away…… Rob waved good bye to Patty as she drove away to the airport to attend a one week conference. Now that she was a prof and he a grad student
When I was learning about solder, I was very surprised when I received a call inquiring about fluxless soldering. Trulyproviding a goodsolder jointwithout using flux; pretty selfexplanatory. Ever
Two categories of solder are available to choose from when the in-service environment for a device reaches above 125°C either in continuous operation or thermal cycling accelerated life
Indium and indium-containing alloys see wide use in a multitude of soldering applications. Indium has many attractive properties such as remaining ductile at cryogenic temperatures, compatibility
I have been asked on numerous occasions to calculate the potential for galvanic corrosion between metals.Most times, when I am approached with this, the concern stems from an application in which the
The use of gold layers deposited onto nickel is standard in many industries, from DRAMmemory module edge connectors, to electrical test probe contacts, to power semiconductor die metallizations and
Eutectic Gold Tin (AuSn) with a composition of 80Au20Sn is a unique material. This particular alloy of gold tin (AuSn) is considered a solder because it has a melting temperature of 280ºC, which
The demand for hermetic packages that house laser diodes is growing, and companies that traditionally made RF/microwave packages are now expanding their businesses into optical packages. What makes
Dr. Ronald C. Lasky: Indium Corporation's Ed Briggs had the great idea to write a paper on the many applications of solder preforms. He asked me to edit and review the paper; the title was The