Indium Corporation is a supplier of specialty solder and brazing spheres in small to mid-size volumes. We offer a wide variety of alloys and sizes from around 0.004” (100 microns) to 0.078” (1.98mm), depending on the alloy. Melting points range from below 90°C to over 700°C.

Powered by Indium Corporation

  • Low-Oxide Sphere
  • Tight Diameter Tolerance Control
  • Tight Alloy Composition Control
Microscopic view of uniform, spherical particles arranged on a dark background.

Features & Benefits

We supply many of the leading suppliers of medical, transportation and automotive, military and aerospace, high-end mobile devices, and computing equipment.

Our customers come to us because we can supply consistently high-quality materials for precision assembly challenges.

  • Accurate diameters
  • Wide range of alloys (<90°C to >700°C)
  • Capable of supplying quantities from 1 sphere to >20 million per month
  • Clean manufacturing and processing ensures low-oxide levels with no organic contamination
  • Whiteroom finishing and packaging ensures continuity of cleanliness
  • Pure metals ensure high-quality finished spheres
  • Manufactured in IATF-16949 certified facilities

Pb-Free Alloys

AlloyIndalloy® #Melting Point
Solidus (°C
Melting Point
Liquidus (°C)
Min
(Inches)*
Max
(Inches)*
Min
(µm)*
Max
(µm)*
InSn5011181250.0040.030102762
InSn48
(In/Sn eutectic)
1E1180.0040.035102889
BiSn42
(Bi/Sn eutectic)
2811380.0080.1092032,769
BiSn42Ag12821391400.0080.030203762
99.99In
(“Pure Indium”)
41570.0040.0501021,270
SnIn20Ag2.8
(Pb-free “Sn63”)
2271751870.0040.030102762
SnAg3Cu0.5
(SAC305)
2562172200.0040.0651021,651
SnAg4Cu0.5
(SAC405)
25622172250.0040.035102889
SnAg41212212280.0040.021102533
SnAg51322212400.0040.032102800
AuSn20
(Au/Sn eutectic)
1822800.0040.039102991

*Approximate Manufacturable Diameter Range

Pb-Containing Alloys

AlloyIndalloy® #Melting Point
Solidus (°C
Melting Point
Liquidus (°C)
Min
(Inches)*
Max
(Inches)*
Min
(µm)*
Max
(µm)*
SnPb46Bi82401601730.0100.030254762
SnPb36Ag2
(Sn62)
Sn621791810.0040.030102762
SnPb37
(Sn63)
1061830.0040.0501021,270
PbIn251101831920.0040.027102686
PbIn402061972310.0040.020102508
PbSn101592753020.0040.0401021,016

*Approximate Manufacturable Diameter Range

Product Data Sheets

Specialty Solder Spheres PDS 97549 (A4) R8.pdf
Specialty Solder Spheres PDS 97549 R8.pdf

Related Applications

Close-up of a square semiconductor chip with four subdivided sections on a green and black background.

Flip-Chip

A crucial technique in advanced semiconductor packaging.

SiP & Heterogeneous Integration Assembly (HIA)

SiP & Heterogeneous Integration Assembly (HIA)

System-in-package (SiP) and heterogeneous integration solutions

Two green microprocessor chips with one showing a grid of pins and the other displaying a central metallic square on a dark surface.

Ball-Attach

Including both water-wash and no-clean ball-attach fluxes

A close-up of a computer microchip with a metallic surface and visible internal components, showcasing advanced 2.5D packaging technology.

2.5D & 3D Packaging

Techniques to incorporate multiple dies in a…

Microchips on a printed circuit board

PCB Assembly

Proven and cutting-edge materials for PCB assembly…

Close-up of several industrial needles with a green blurred background.

Rework

Our rework solutions include solder wire, TACflux,…

Related Markets

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.