Products Thermal Interface Materials Liquid Metal and Liquid Metal Paste

Liquid Metal and Liquid Metal Pastes

Indium Corporation’s liquid metals are pure metals, or metal alloys, that remain liquid at room temperature, with melting points between 7.6°C and 17°C. These alloys are primarily gallium-based, often combined with elements like indium, tin, or zinc. All our liquid metals are RoHS-compliant, non-toxic, and can be transported globally in full compliance with shipping regulations.

Liquid Metal Properties

  • Liquid at Room Temperature
  • High Thermal Conductivity
  • Non-Toxic, Gallium-Based Materials
Close-up of a CPU chip with thermal paste dots applied, ready for a heatsink.

Liquid metals wet to most metallic and non-metallic surfaces through two mechanisms—oxide pinning, a physical bond of an oxide to a relatively smooth surface, and reactive wetting, a metallurgical bond.

Gallium-based metals have excellent thermal conductivity, making them an ideal thermal interface material. As high-density, low viscosity materials, these substances form a thin, self-limiting oxide layer on their surface when exposed to air.

Another interesting property of gallium-based liquid metals is that their thermal conductivity increases with temperature, meaning that the thermal performance of liquid metal TIMs improves as well.

Liquid metals are electrically conductive and must be contained to prevent leakage or shorts in electronics. Indium Corporation’s patented multi-barrier system ensures compatibility, corrosion resistance, flexibility, and durability with gallium-based materials.

Indium Corporation’s Patented Multi-Barrier System for Liquid and Hybrid Liquid Metals

Diagram showing a heat-sink above a substrate with a die, TIM, and spacers B1 and B2 labeled h1.
Dark green icon with stylized shapes and a dot on a white circular background.

High-Density, Low Viscosity

Dark green icon with stylized shapes and a dot on a white circular background.

Non-Toxic Alternative to Mercury

Dark green icon with stylized shapes and a dot on a white circular background.

Flexible and Stretchable Electronics

Dark green icon with stylized shapes and a dot on a white circular background.

Excellent Thermal and Electrical Conductivity

Liquid Metal and Liquid Metal Paste Products

Product Data Sheets

Liquid Metal Gallium and Gallium Alloys PDS 97826.pdf
Liquid Metal TIMs PDS 99939 R2.pdf
m2TIM® and Liquid Metal Thermal Interface Materials PDS 99600 R4.pdf

Related Applications

Liquid metal and liquid metal paste products are suitable for a variety of applications.

Close-up of a computer microchip on a green circuit board with visible electronic components and patterns.

Thermal Management

Thermal solutions for HPC ensuring reliability and…

Illustration of a microchip with a transparent overlay, revealing internal components and electronic connections, highlighting the precision akin to a tim1 40 design.

TIM1, TIM1.5, TIM2

Metal-based TIMs deliver high thermal performance and…

Related Markets

Indium Corporation’s liquid metal and liquid metal paste products are available for use in a wide range of markets.

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.