Indium Corporation is a leading gold solder innovator for high-temperature and high-reliability applications, such as die-attach and hermetic sealing in medical, aerospace, optoelectronics, automotive, and many other industries.
Gold-based alloys offer strong joints, excellent corrosion and oxidation resistance, and good thermal and electrical transfer at the joint. Our gold solder portfolio includes wire, paste, preforms, and ribbon. They are manufactured with cutting-edge technology to ensure quality as well as push the boundaries of precision.
Higher yields and cost per unit make gold a viable option for many applications, even though the initial cost is more than alternative solders. A low oxygen atmosphere may be required if the application is flux free. In some instances, pressure is required to promote strong, void-free reflow on horizontal services.
Attributes
Gold solder is known for strong bond strength, excellent corrosion and oxidation resistance, and reliable thermal and electrical transfer at the braze joint.
Processing Options
Choose from proven processing methods, including: vacuum soldering, die-attach, reflow, laser soldering, vapor phase reflow, and manual soldering.
Features
We offer more than 320 alloy solutions capable of withstanding temperatures up to 1,100°C. Innovative lead-free alternatives—including gold solders, sintering, preforms, and advanced alloy technologies integrated with new flux systems—are also part of our ongoing development efforts.
>280°C
High melting point compatible with subsequent reflow processes.
Critical Applications
Automotive, RF infrastructure, medical, laser, military, and aerospace applications.
Pb-free
Lead-free and RoHS compliant.
#1 in Reliability
Highest tensile strength of any solder.
Gold-Based Alloys
Indium Corporation offers a broad range of gold-based alloy solutions with melting temperatures up to 1,064°C:
Alloy Name
Composition
Melting Point
Indalloy®182
80Au20Sn
280°C Eutectic
Indalloy®200
100Au
1,064°C Eutectic
Indalloy®178
82Au18In
Solidus 451°C / Liquidus 485°C
Indalloy®184
96.8Au3.2Si
363°C Eutectic
Indalloy®183
88Au12Ge
356°C Eutectic
Indalloy®270
75Au25Sn
Solidus 278°C / Liquidus 332°C
Indalloy®269
78Au22Sn
Solidus 278°C / Liquidus 301°C
Indalloy®271
79Au21Sn
Solidus 278°C / Liquidus 289°C
Gold Solder Products
With years of experience in the industry, we have built a strong foundation of knowledge and expertise in solving manufacturing challenges. We provide a wide array of alloys and flux choices, leveraging our technical proficiency to act as a strategic ally for each client, ensuring the delivery of exceptional results and performance.
Indium Corporation is a leading gold solder innovator for high-temperature, high-reliability, and critical applications such as die-attach and hermetic sealing in:
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!
Interconnect reliability is critical to the reliability of semiconductor packaging and electronic systems. If we look at the life cycle from the chip to the system—from IC design, wafer fab,
Folks, This post is an excerpt on graping, fromIndium Corporation'sThe Printed Circuits Assemblers Guide to Solder Defects. Introduction The growth of personal electronic devices continues to
In history, “The Gold Standard” was a monetary system in which countries fixed their currencies to a specified amount of gold. Here at Indium, we also use the phrase, however, to
When we talk about off-eutectic alloys, we must take a step back and talk about what makes a eutectic alloy. Each solder alloy has both a solidus (not melted) and liquidus (completely melted)
Folks, It's been way too long, let's look in on Patty and the boys….. It was 5:30AM and Patty’s alarm went off. She was unusually tired today because of a PTA meeting last
Folks, Some years ago I received the request below: Hi Dr. Lasky, I am a precious metals recycler and would very much appreciate your verifying the validity of an equation that approximates the Karat
We have had a chance to look at low-temperature solder alloys and indium in particular. Now it is time to look at high-temperature solder and braze alloy options. Bernie Leavitt is our Senior Product
Dr. Ronald C. Lasky: Indium Corporation's Ed Briggs had the great idea to write a paper on the many applications of solder preforms. He asked me to edit and review the paper; the title was The
The demand for hermetic packages that house laser diodes is growing, and companies that traditionally made RF/microwave packages are now expanding their businesses into optical packages. What makes