Produtos Ligas Ligas fusíveis/Ligas de baixo ponto de fusão

Ligas fusíveis/Ligas de baixo ponto de fusão

Fusible alloys, known for their lower melting points compared to solder alloys, are easily liquefied with moderate heat, making them ideal for temporary solid state during processing or as temperature sensors, such as in fire detection sprinkler systems. Originally developed in the 19th century and known by names such as Field’s metal, Wood’s metal, and Rose’s metal, these alloys have evolved with modern materials technology to include precise compositions like Indalloy®117, Indalloy®158, and Indalloy®19, delivering consistent melting behavior across an extended temperature range.

Desenvolvido por Indium Corporation

  • Broad Alloy Portfolio and Formulation Depth
  • Materials Science and Process Support
  • Leading Global Supplier of Fusible Alloys
Lens Blocking using Fusible Alloys
Lens Blocking using Fusible Alloys or Low Melting Point Alloys

Visão geral do produto

Fusible alloys, characterized by their low melting points as low as 47°C (117°F), offer remarkable versatility by transitioning seamlessly between solid and molten states. This unique property makes them indispensable for precise and temporary applications. These alloys serve as excellent as precision support materials, securely holding and protecting workpieces during crucial finishing processes, such as polishing and grinding. Additionally, the eutectic melting points of fusible alloys facilitate passive activation systems, ensuring the reliable and safe operation of devices like fire sprinklers without the need for electronic circuitry, thereby enhancing safety and simplicity.

A maior gama de composições de ligas disponíveis

Field’s metal, Wood’s metal, and many other alloy compositions are available. Available melting points start at 47°C/117°F and go up into the solder alloy range at above 200°C.

Lens Blocking for Grinding and Polishing with Indalloy®117 & Indalloy®19

Indalloy®117 and Indalloy®19 are the most popular alloys for lens blocking in the optical lens grinding industry, with melt points at 47°C/117°F and 60°C/140°F, respectively.

Ativação precisa de sistemas de sprinklers contra incêndios

Melting activation is solely controlled by environmental temperature and thus enables the design of completely passive devices for fire detection. Indalloy®158 is a popular alloy choice for fire sprinkler systems.

Custom Alloy Development

Melting behavior is determined by precise control of the alloy composition. We offer a wide range of alloy options and melting points. We also work with customers to develop custom alloys with target melting points and other properties tailored to their application needs.

Indalloy®117

Indalloy®19 (Field’s Metal)

Indalloy®158 (Wood’s Metal)

Opções de ligas sem chumbo e cádmio

Indalloy #11713619158281
Composição da liga44,7 Bi
22,6 Pb
19,1 In
8,3 Sn
5,3 Cd
49 Bi
21 In
18 Pb
12 Sn
51 In
32,5 Bi
16,5 Sn
50 Bi
26,7 Pb
13,3 Sn
10 Cd
58 Bi
42 Sn
Liquidus em °C (°F)47 (117)58 (136)
60 (140)

60 (140)

138 (281)
E = EutécticoEEEEE

Aplicações relacionadas

As ligas fusíveis/ligas de baixo ponto de fusão são adequadas para uma vasta gama de aplicações.

Microchips numa placa de circuito impresso

Montagem de PCB

Materiais comprovados e de ponta para montagem de PCB...

Soldadura a alta temperatura

Soldadura a alta temperatura

Offering high-temperature soldering materials for critical applications…

Cilindro preto texturado com selos criogénicos, com três etiquetas rectangulares brancas no topo.

Vedação: criogénica e hermética

Low temperature liquid & fusible alloys for…

Mercados relacionados

As ligas fusíveis/ligas de baixo ponto de fusão da Indium Corporation são adequadas para muitos mercados.

Tem perguntas técnicas ou questões de vendas? A nossa equipa dedicada está aqui para ajudar. "From One Engineer to Another®" não é apenas o nosso lema - é o nosso compromisso de prestar um serviço excecional. Estamos prontos quando você estiver. Vamos ligar-nos!

Esta imagem tem um atributo alt vazio; o seu nome de ficheiro é scientist-with-microscope.png

Procura fichas de dados de segurança?

Aceda a tudo o que precisa - desde especificações técnicas a orientações de aplicação - numa localização conveniente.