Products Compounds Indium Tin Oxide (ITO)

Indium Tin Oxit (ITO)

Indium tin oxide (ITO) is a composite material consisting of indium(III) oxide (In₂O₃) and tin (IV) oxide (SnO₂), typically in a 90:10 weight ratio. Known for its exceptional transparency and low sheet resistance, ITO is a preferred choice for flat panel displays and touch sensors. Indium Corporation offers premium, high-purity ITO products in bulk, suitable for fabricating sputter targets or creating ink formulations. Our ITO is provided in powder form, which can be compressed and sintered into sputter targets or used to produce ink-like coatings.

Được cung cấp bởi Indium Corporation

  • Flexibility Over the Indium Oxide
  • Tight Control
  • Low Impurities, With a Powder Purity Level of >4N5
Một đống bột trắng mịn, tiền chất của oxit thiếc indi, nằm trong một đĩa petri thủy tinh trong suốt trên nền tối.

While the 90/10 ratio of indium oxide to tin oxide is commonly preferred, we also offer alternative ratios to meet diverse needs. Our formulations range from 87% to 95% indium oxide by weight, enabling precise customization of sheet resistance and transparency in deposited films to suit specific customer requirements.

Our powder particles are precisely controlled to ensure a consistent size distribution, which plays a crucial role in the performance of our ITO products. The particle size and BET (surface area per unit mass) are closely related, and we carefully manage the BET value throughout our processes. We also provide this information with every shipment to support optimal performance in your applications.

Metallic impurities can greatly affect the electronic and optical performance of ITO films. We enforce stringent controls to minimize these impurities and provide detailed documentation of their levels in the Certificate of Analysis (COA) for each shipment.

Dark green icon with stylized shapes and a dot on a white circular background.

Mobile phones

Dark green icon with stylized shapes and a dot on a white circular background.

Balanced ratio

Dark green icon with stylized shapes and a dot on a white circular background.

80%

Dark green icon with stylized shapes and a dot on a white circular background.

4 eV

Loại sản phẩmd90d50d10BET m2/g (typical)
Type A – Standard32.0-44.013.2-24.02.7-8.02.4
Type D – Very Fine4.3-11.51.1-3.00.4-0.818.5

Bảng dữ liệu sản phẩm

Oxit Indi-Thiếc (ITO) PDS 97550 R12.pdf

Ứng dụng liên quan

ITO is suitable for a wide range of applications.

Liên kết phân tử cho thấy sự tổng hợp hóa học

Tổng hợp hóa học

Indium and gallium compounds for chemical synthesis…

Thị trường liên quan

Indium Corporation’s ITO is available for use in the following markets:

Bạn có thắc mắc về kỹ thuật hoặc yêu cầu bán hàng không? Đội ngũ tận tâm của chúng tôi luôn sẵn sàng trợ giúp. “Từ kỹ sư này đến kỹ sư khác®” không chỉ là phương châm của chúng tôi—mà còn là cam kết của chúng tôi trong việc cung cấp dịch vụ đặc biệt. Chúng tôi luôn sẵn sàng khi bạn sẵn sàng. Hãy kết nối!

Hình ảnh này có thuộc tính alt trống; tên tệp của nó là scientific-with-microscope.png

Bạn đang tìm kiếm Bảng dữ liệu an toàn?

Truy cập mọi thứ bạn cần — từ thông số kỹ thuật đến hướng dẫn ứng dụng — tại một vị trí thuận tiện.