Saltar para o conteúdo

Indium Corporation’s Technology Experts to Present at SMTA/iNEMI

Indium Corporation’s Dr. Ning-Cheng Lee, Vice President of Technology, and Dr. Ron Lasky, Senior Technologist, will present at the SMTA/iNEMI Medical Electronics Symposium November 13-14 in Milpitas, California.

Dr. Lee’s presentation, Shock Resistant and Thermally Reliable Low-Ag SAC Solder Doped with Mn for Portable Medical Devices, discusses a new soldering alloy doped with Mn, and its considerable improvement in shock resistance and thermal fatigue performance.

Dr. Lasky’s presentation, Tin Whiskers: Causes, Risks, and Mitigation, reviews what tin whiskers are, how they form, mitigation techniques, and how to use failure modes and effects analysis as techniques to assess tin whisker risk.

Dr. Lee is a world-renown soldering expert and an SMTA Member of Distinction. He has extensive experience in the development of high-temperature polymers, encapsulants for microelectronics, underfills, and adhesives. His current research interests include advance materials for interconnects and packaging for electronics and optoelectronics applications, with an emphasis on both high performance and low cost of ownership.

Dr. Lasky, holder of the prestigious SMTA Founder’s Award, is a world-renown process expert and an Instructional Professor at Dartmouth College. He has over 30 years of experience in electronics and optoelectronic packaging and assembly. He has authored or edited five books and numerous technical papers and holds several patent disclosures. Dr. Lasky also authors a technology blog, which can be found at indiumstg.wpenginepowered.com/drlasky.

A Indium Corporation é um fabricante e fornecedor de referência de materiais para os mercados globais de eletrónica, semicondutores, energia solar, películas finas e gestão térmica. Os produtos incluem soldas e fluxos; ligas de brasagem; materiais de interface térmica; alvos de pulverização catódica; metais e compostos inorgânicos de índio, gálio, germânio e estanho; eNanoFoil®. Fundada em 1934, a Indium dispõe de apoio técnico global e fábricas localizadas na China, Singapura, Coreia do Sul, Reino Unido e EUA.

Para mais informações sobre a Indium Corporation, visite indiumstg.wpenginepowered.com ou envie um e-mail para [email protected].