Indium Corporation will showcase its innovative Durafuse technology at the EPP InnovationsFORUM on Tuesday, June 28 in Leinfelden-Echterdingen, Germany.
The harmful effects of lead on human health and the environment are driving the development of high-temperature lead-free (HTLF) solders to replace high-Pb solders for die-attachment and clip-bond in power device applications. Indium Corporations innovative Durafuse HT features a novel design based on a mixed-alloy technology, designed to deliver a tin-rich HTLF paste, presenting the merits of both constituent alloys. Durafuse HT delivers:
- Simplified processing; Durafuse HT is a drop-in replacement for high-Pb solder, with no special equipment needed and minimal process adjustments
- Enhanced thermal cycling reliability; equal or higher than high-Pb solder
- Lower RDS(on) compared to high-Pb solder
Indium Corporations award-winning Durafuse LT is a patented low-temperature alloy system designed to provide high-reliability in low-temperature applications that require a reflow temperature below 210C. Durafuse LT delivers:
- Improved drop shock performance more than two orders of magnitude better than Bi-containing low-temperature materials
- Drop shock performance equal or better than SAC305 with proper process optimization
- Ideal characteristics for step soldering and low-temperature requirements
Sobre a Indium Corporation
A Indium Corporation é um dos principais refinadores, fundidores, fabricantes e fornecedores de materiais para os mercados globais de eletrónica, semicondutores, película fina e gestão térmica. Os produtos incluem soldas e fluxos; brasagens; materiais de interface térmica; alvos de pulverização; metais e compostos inorgânicos de índio, gálio, germânio e estanho; e NanoFoil. Fundada em 1934, a empresa tem apoio técnico global e fábricas localizadas na China, Alemanha, Índia, Malásia, Singapura, Coreia do Sul, Reino Unido e EUA.
Para mais informações sobre a Indium Corporation, visiteindiumstg.wpenginepowered.comou envie um e-mail paraJingya Huang. Também pode seguir os nossos especialistas, «From One Engineer To Another»(#FOETA), emwww.linkedin.com/company/indium-corporation/ou@IndiumCorp.
About EPP InnovationsFORUM
The EPP InnovationsFORUM is the leading, independent event in the field of manufacturing electronic assemblies. Click here to learn more.