Indium Corporation to Showcase Durafuse Technology at EPP InnovationsFORUM

Indium Corporation will showcase its innovative Durafuse technology at the EPP InnovationsFORUM on Tuesday, June 28 in Leinfelden-Echterdingen, Germany.

The harmful effects of lead on human health and the environment are driving the development of high-temperature lead-free (HTLF) solders to replace high-Pb solders for die-attachment and clip-bond in power device applications. Indium Corporations innovative Durafuse HT features a novel design based on a mixed-alloy technology, designed to deliver a tin-rich HTLF paste, presenting the merits of both constituent alloys. Durafuse HT delivers:

  • Simplified processing; Durafuse HT is a drop-in replacement for high-Pb solder, with no special equipment needed and minimal process adjustments
  • Enhanced thermal cycling reliability; equal or higher than high-Pb solder
  • Lower RDS(on) compared to high-Pb solder

Indium Corporations award-winning Durafuse LT is a patented low-temperature alloy system designed to provide high-reliability in low-temperature applications that require a reflow temperature below 210C. Durafuse LT delivers:

  • Improved drop shock performance more than two orders of magnitude better than Bi-containing low-temperature materials
  • Drop shock performance equal or better than SAC305 with proper process optimization
  • Ideal characteristics for step soldering and low-temperature requirements

Sobre a Indium Corporation

A Indium Corporation é um dos principais refinadores, fundidores, fabricantes e fornecedores de materiais para os mercados globais de eletrónica, semicondutores, película fina e gestão térmica. Os produtos incluem soldas e fluxos; brasagens; materiais de interface térmica; alvos de pulverização; metais e compostos inorgânicos de índio, gálio, germânio e estanho; e NanoFoil. Fundada em 1934, a empresa tem apoio técnico global e fábricas localizadas na China, Alemanha, Índia, Malásia, Singapura, Coreia do Sul, Reino Unido e EUA.

For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email Jingya Huang. You can also follow our experts, From One Engineer To Another (#FOETA), at www.linkedin.com/company/indium-corporation/ or @IndiumCorp.

About EPP InnovationsFORUM

The EPP InnovationsFORUM is the leading, independent event in the field of manufacturing electronic assemblies. Click here to learn more.