Anytime something cold is introduced into a warm/humid environment it will collect droplets of water from the surrounding air. Since substrate bumping paste is stored cold, please remember to let it warm up to ambient temperature before removing the lid of the jar.
Beware Condensation on Substrate Bumping Paste
Indium Corporation Blogging Team
Our blogging team includes engineers, researchers, product specialists, and industry leaders. We share expertise in solder materials, electronics assembly, thermal management, and advanced manufacturing. Our blog offers insights, technical knowledge, and solutions to inspire professionals, showcasing product innovations, trends, and best practices to help readers excel in a competitive industry.