Indium Solder for Heat Sensitive Components

Are you looking for a solution to soldering heat sensitive components? If traditional soldering temperatures are too hot, consider using low-temperature indium alloys instead. With liquidus temperatures between 118-187°C (and some even lower), indium alloys can help you reduce your assembly temperature. These alloys come in all the forms you arefamiliar withfor traditional alloys, including solder paste, wire, ribbon, washers, frames, discs, rectangles, and special shaped preforms.