Blog

Support

Meet The Bloggers – Round 2

We had a pretty good turnout at Semicon West 2008 with our first “Meet the Bloggers” event, so we decided to try doing a similar thing for SMTAI Aug. 20th. The team has devised a list of

Products

Join Me at SMTAI

One of the electronics largest trade shows of the year, SMTAI is nearing on the week of August 18th.At this show in Orlando, Florida, Tim Jensen and I will be presenting a paper titled,

Products

Filling in the Gaps

To see your process as a whole, you need to really understand your materials. I’ve known companies that teach us a thing or two about materials, but I’ve also worked with engineers who

Products

Thermal Interface Materials

Liquid Metal Thermal Interface Materials Dispensing Thermal Grease. Image Courtesy of

Products

An Interview with Michael Qiu 采访邱学丞

Michael Qiu supports Indium Corporation in Eastern China. I thought an interview with him would be a good chance to see the semiconductor industry from a different

Products

The Electronics Cooling Industry – Pushing the Creative Limits!!!

Celsia Technologies, an established name in the electronics cooling market for their advanced heat spreaders recently unveiled an advertisement in Electronics Cooling Magazine which was unlike others

Products

Solder Alloy Density Calculator

Looking for the density of a solder alloy? Many of you already know the density equation for an alloy, but if you want a quick way to do this simple calculation, you can use Indium's Solder Alloy

Products

Hardly Scrap – The Silicon Market

Are you giving away your broken and mis-registered wafers? …Probably not, if you realize the value of those thin silicon treasures. For those of us who like to work with unique wafers, finding

Sales

New B2B Marcom Newsletter

Terri Rylanderhas established a monthly B2B Marcom newsletter to discuss "content development, design, writing tips, the sales & marketing cycle, and freelance ideas." The

Products

Alloy Density Calculator Goes Live

Folks, Over the past few years I have been surprised at the interest in the Excel based alloy density calculator that I developed. Thanks for your interest! In light of this interest, team Indium

Products

Thermal Temperature Cycling of Indium Alloys

To quantify reliability parameters, accelerated life tests are performed on electronic devices, including all thermal materials, including thermal interface materials. Most new materials are

Products

Stock Up

I recently visited a customer to help optimize a flux-less indium soldering application. They admitted they needed flux but didn’t know 1) what to use, or 2) if there was a better way to fix

Products

Indium’s M&C Business Unit (Indium公司的金属与化学品事业&#3709

Indium solar material 1 Indium solar material 2 Korean delicate Kimchi Indium 公司有两个事业部,Solder Material Business Unit 和 Metal & Chemical Business Unit.

Products

Are You A Star? – You Can Be

We’re always looking for something new, so I thought I’d ask you (the best blog audience out there) first. Would you like to be part of an Indium materials processing video? Here’s

Products

Rick Short at Semicon West 2008

Learn from Rick how this whole Indium Blogging thing started.

Sales

Dr. Ron Gets Second Eagle in Golf in a Year

Folks, Lest I seem braggy, one thing must be made clear. In general I have never been a good athlete. I can not get my body coordinated enough to make a "layup" in basketball, and I was

Archive

世界给我十六天,我还世界五千年!—Counting Down for the 2008 Beijing Olympic Games!

Beijing National Grand Theather 北京大剧院 Bird’s Nest 鸟巢 Beijing National Olympic Swimming Center 水立方 上周末在纽约市度过。在曼哈顿唐人街(Manhattan Chinatown)

Support

Andy Mackie at Semicon West 2008

Although Andydoesn’t directly blog, learn how he helps with this and other blogs. We will be seeing more video installments of Dr. Andy Mackie (pictured, right) soon.

Products

Paul Socha at Semicon West 2008

Paul describes how he contributes to the Engineered Solders Blog while at the show. Click here to view the video. If you haven’t already, I suggest visiting the Engineered Solders Blog. Not

Products

Die Size Vs. Temperature Cycles to Failure

Solder TIMs are the bonding and joining material used to connect small, powerful dies to their substrates. Some of these dies are exposed to severe temperature conditions which cycle into opposite

Products

Pin Transfer Basics

This is the shape of flux deposits left after pin transfer Spheres attached after pin transfer Pin transfer is a way of selectively depositing a semi-solid or liquid material (like a solder paste or

At Indium we research, develop, and manufacture advanced electronics assembly materials solutions to the challenges of today, tomorrow, and the future.